Kabòn Steel A234 WPB San pwoblèm koud 90 Degre LR
Estanda: ASME B16.9
Klas: ASTM A234 WPB
Kalite: Long Radius
Ekspozisyon pwodwi yo


Pwodwi Deskripsyon
|
Non pwodwi |
Kabòn Steel A234 WPB San pwoblèm koud 90 Degre LR |
|
Estanda |
ASME B16.9 |
|
Klas |
ASTM A234 WPB |
|
Angle koud |
90 degre |
|
Kalite |
Reyon Long (LR), Reyon Bend=1.5D |
|
Pwosesis Pwodiksyon |
Cho pouse/Extrusion |
|
Kalite Koneksyon |
BW |
|
Gwosè Range |
NPS 1/2 "~ 48" / DN15 ~ DN1200 |
|
Epesè |
SCH 40 (STD), SCH 80 (XS), SCH 160, XXS |
|
Sifas |
Nwa Anti-penti rouye, vèni, sablaj (Personalize) |
|
Sètifikasyon |
ISO 9001, SGS, BV (Disponib sou demann) |
Tablo konparezon gwosè komen
|
NPS (pous) |
DN (Dyamèt nominal) |
Dyamèt ekstèn OD (mm) |
Sant pou bout longè A (mm) |
|
1/2" |
15 |
21.3 |
38 |
|
3/4" |
20 |
26.7 |
38 |
|
1" |
25 |
33.4 |
38 |
|
1-1/4" |
32 |
42.2 |
48 |
|
1-1/2" |
40 |
48.3 |
57 |
|
2" |
50 |
60.3 |
76 |
|
3" |
80 |
88.9 |
114 |
|
4" |
100 |
114.3 |
152 |
|
6" |
150 |
168.3 |
229 |
|
8" |
200 |
219.1 |
305 |
Konpozisyon chimik materyèl (analiz k ap fonn)
|
Eleman |
C |
Mn |
P |
S |
Si |
|
Limit kontni/Gamme |
Mwens pase oswa egal a 0.30% |
0.29~1.06% |
Mwens pase oswa egal a 0.05% |
Mwens pase oswa egal a 0.058% |
Mwens pase oswa egal a 0.40% |
FAQ
K: Ki diferans ki genyen ant 90 degre LR ak SR koud? Ki jan yo chwazi?
A: LR: 1.5D reyon koube, rezistans ki ba / pèt presyon ki ba, estanda pou tiyo endistriyèl; SR: 1.0D, kontra enfòmèl ant men rezistans segondè, sèlman pou tiyo segondè presyon ba - ak espas limite.
K: Ki sa ki ASTM A234 WPB? Ranje tanperati aplikab?
A: US estanda asye kabòn fòje, inivèsèl pou ekipman endistriyèl; Tanperati aplikab: -29 degre ~ 425 degre. Chwazi A420 WPL6 pou tanperati ki ba, WP11/WP22 pou tanperati ki wo.
Baj popilè: kabòn asye a234 wpb san pwoblèm koud 90 degre lr, Lachin asye kabòn a234 wpb san pwoblèm koud 90 degre lr manifaktirè, Swèd, faktori